1 Questions 1 Answers 0 Followers
Questions related from Onur Tüfekci
I am using TSG-250 solution.Deposited area is 7.5 cm2, pulse mode %10 duty cycle, 20mA, tempature 50 cel. and strring 200 RPM. This recipe give me roughness surface.How can I develop this recipe?
05 May 2017 2,570 3 View