5 Questions 14 Answers 0 Followers
Questions related from Michele Miliciani
by my lab experience there is no compatibility printing a polyester based ink on polycarbonate substrates, cracks occurs after drying step. any chance to add an additive (wetting agent,...
29 July 2021 9,105 3 View
It is well known that adding PEG or other glycols reduce the sheet resistance in polymeric formulations based on micro size silver particles. What is the model approach to understand the...
01 July 2021 2,412 3 View
the goal is to produce a UV transparent dielectric composition with no "white" pigment added but with a good dielectric strength (>1000V@25mic printed thickness). how to realize so high...
25 June 2021 5,228 3 View
how to increase the elongation @break for the polycaprolattone ? PCL was used in thermoforming applications and needs to improve elongation @break to avoid cracks after forming step. Some...
17 June 2021 2,191 8 View
In order to improve the intimate contact of micro size silver flake in a solvent based printable polymer conductor I am looking for a method to precipitate nAg powder (from Ag salts) on an...
14 December 2020 6,598 4 View