Can you guide me about this topic? I have a sample with 180 HV (HV0.3), which consists of coarse and fine pits of different depths, and I want to check local hard zones possibility by measuring...
27 February 2024 7,510 7 View
Hi Is there any criteria value for banded (microstructure) rate?
30 April 2023 8,466 1 View
I read papers that their method was design the melting preparation, but when we did those process, not get good result (it did not work well)! We want to reduce Fe in AZ61 alloys lower of 50 ppm.
26 May 2021 1,320 2 View
What's your suggestion for selecting the material with high electrical conductivity and high specific area? Thank you
07 May 2021 8,188 9 View