Hi everyone,For an aqueous slurry of weight 500g (water+binder+ceramic), what is a reasonable duration for rolled ball-milling before spray-drying?At what would be a recommended speed of...
03 March 2015 9,559 13 View
HiCan anyone tell me whether there are any labs that offer materials characterization services at reasonable cost in Asia? I have the physical properties of some ceramic powders to investigate...
03 March 2015 1,209 7 View
Hi everyone, I'm confused about nanostructured coatings. Say I have a material those grain size is of micron order ~ 10um, but consists of primary nanosized particles ~3nm and mean pore diameter...