Questions related from Laura Manenti
Hi all, Are there non-destructive ways to measure the thicknesses of the bilayers made of SiO2 and Si3N4 in a multilayer stack? I have 23 bi-layers, for a total thickness of about 11 um. I was...
15 July 2021 3,322 4 View
Hi, In June 2018 I made a batch of Silver film depositions on Si plates. At the time, I used a A306 Metal Box Evaporator, 3 cm of 99.99% Silver wire. As of today (03.04.2019) there is no visible...
03 April 2019 8,334 5 View
I am currently using a Xe-flash lamp (200-2000 nm spectrum) to extract electrons from a gold plate (~100 nm deposition). Gold has a work function of around 5.1 eV (~245 nm) and does not oxidise....
07 May 2018 2,710 5 View