The reference electrod I use is saturated calomel electrode (3M KCl as the filling solution). I got overload problem while measuring the EIS, so then I checked the impedance of the electrod and...
28 May 2020 7,766 12 View
We observe some cracks among the nanotubes which are formed on the surface of the Ti alloy after anodic oxdation. What could be the cause of this problem?