1 Questions 1 Answers 0 Followers
Questions related from Heesang Ahn
We want to make gold film(40nm) on the BK7 using the adhesive material Cr(2nm). Here's my work order. First, we evaporate the Chromium on the glass(BK7) by thermal evaporator with 0.2 A/sec.(when...
08 October 2014 5,418 5 View