Questions related from Hassan Saleem Agiwaan
Hi, I am performing cross-section preparation of tungsten wires of diameters 345, 155, 64, 41 µm by mechanical grinding and polishing. I am using SiC foils of different grit sizes. For coarse...
01 July 2017 6,670 4 View
In case of TiAlN coatings with high Al >70% contents appeared to be x-ray amorphous i.e., showed no phases all the way from as-deposited condition to annealed to 1100 degree celsius while showed...
29 October 2013 8,582 25 View