Hi all an easy question: in tube hydroforming process when the axial feed parameter is for example 6mm ; is it mean that we have 6mm axial feed to both sides of tube or 6mm is applied to all of...
09 September 2016 1,367 2 View
Hi im simulating hydroforming process in abaqus. this process has two major limitations: Bursting and Wrinkling. for bursting criterion, it can be used from FLD (Forming Limit Diagrams) or FLSD in...