7 Questions 2 Answers 0 Followers
Questions related from Emmanuel Nwaogu
Hello, I'm working on V2C Mxene. and V2AlC Maxphase. Please who can tell me the theoretical capacities of these materials above I can not get good cycling capacity after charge-discharge. I think...
18 August 2023 1,766 0 View
for example, how to make some like 3.8-14.6 mg cm-2?
06 December 2022 5,550 1 View
For example: 0.4 mA h /cm2 of lithium was deposited on copper foam on current density of 10 mA/ cm2
25 November 2022 549 0 View
For example Then 1 mAh cm−2 of Li was plated on the current collector at a current density of 1 mA cm−2 and the cutoff potential for the discharge process was set to 1.0 V.
25 November 2022 1,869 0 View
In my project i want to check the amount of lithium is able to deposit on the cu current collector after plating using Biologic tester or any other tester.
08 November 2022 2,083 1 View
Please how can i prepare my electrolyte with respect to the amount of solvent. For example how much solvent is required to prepare 3M of LPF6 lithium salt with EC/EMC (1:2 v/v) solvent?
01 January 1970 6,897 2 View
How can one control the capacity loading of Li at 0.1 mAh /cm2 with a current density at 10 μA /cm2 using Biologic Tester or Galvano static tester
01 January 1970 4,710 0 View