3 Questions 8 Answers 0 Followers
Questions related from Debasmita Kandi
I have prepared a metal oxide composite with 2 wt % of GO by hydrothermal method, now I want to know after the reaction what is the amount of RGO has been present in this composite.
13 September 2019 9,074 3 View
I am working on degradation of antibiotics at different pH conditions. I found that degradation rate is maximum at pH 3 and 6 for tetracycline and oxy-tetracycline respectively. At pH 3, both the...
06 June 2019 8,430 3 View
Usually the degradation rate of Rhodamine B follows pseudo first order kinetics. But there is few reported literature zero order kinetics was mentioned. Is it right to follow zero order kinetics ?...
10 November 2017 3,738 12 View