I have performed some high strain rate (in the order of 102-103 s-1) compression tests on Al 7075 samples at different temperatures. I see some twin-shaped grains on the optical images for some of...
06 July 2021 5,212 5 View
The precipitates formed inside the AA7075 material due to T6 heat treatment start to dissolve around 200 degree celsius. The polyplast mounting material that I am using for hot mounting is...