After heating for 10-15 min at 982 Celcius, the Alloy 600 can be cooled either in the air or in water since the softening is independent of quenching rate.
12 March 2020 8,008 2 View
What is the maximum reduction possible through cold=working in zirconium alloy tubes? And what is the annealing temperature to restore the mechanical properties?