09 September 2016 11 3K Report

Often we have oversize of massive elements of casting. This oversize can reach 5 % (look at the picture). This problem looks like material grows (ductile iron). We know that increase of metal volume while it cooling, is impossible. Bat we have it.

One more, when we pour grey iron (without the spheroidising  and  modifying  master  alloy  in  a  reaction  chamber), we will have normal sizes of our casting.

May be someone had similar problem and knows decisions or materials of it?